Properties |
Test
Method (ASTM) |
Typical
Value |
Physical |
| Specific
Gravity |
D792 |
1.073 |
| Mold
Shrinkage |
D955 |
0.006
in/in |
| Colour |
|
Black |
| Melt
Flow Rate |
D1238 |
10.0
g/10mins |
|
Mechanical
|
Tensile
Strength |
Yield |
D638
|
16 MPa |
| Break |
D638 |
12 MPa |
| Tensile
Modulus |
D638 |
1175
MPa |
Tensile
Elongation
|
Yield |
D638 |
1.7 % |
| Break |
D638 |
12.3
% |
Flexural
Strength
|
D790 |
25
MPa |
Flexural
Modulus
|
D790 |
1356
MPa |
Impact
Strength |
D256 |
121.2
J/m |
Thermal |
|
@ 0.45 MPa |
D648 |
73
Degree C |
@
1.84 MPa |
D648 |
72
Degree C |
Electrical |
Surface
Resistivity
|
D257 |
< 10E5 ohm/sq |
Packaging
|
25kg/bag |
25kg/bag |
|
| |
|
|